Matching a Pantone colour on porcelain: glaze, decoration and tolerances

Brands often arrive with a Pantone reference. On porcelain, colour is born in the kiln: it is adjusted through test firings and always approved on a fired piece, never on screen.

Matching a Pantone colour on porcelain: glaze, decoration and tolerances

A colour born in firing

Ceramic colours are mineral pigments that change in the kiln. A shade on the palette does not always look like the final shade: the fired piece is the reference.

Coloured glaze or decoration

A coloured glaze tints the whole surface; a decal applies a logo or a pattern. Each has its own palette and constraints, and is adjusted separately.

Test firings

We start from the Pantone reference, prepare several proposals and fire them on the chosen porcelain. The closest shade is chosen on the piece, in daylight.

Difficult colours

Some very bright or fluorescent shades have no equivalent in ceramic colours. We then look for the closest shade and approve it together.

The base matters

The white of the body, the gloss of the glaze and the firing all influence colour. The same reference can vary slightly from one porcelain to another.

Consistency in production

Once approved, the shade becomes the production reference: each batch is compared with the approved sample.

Can an exact Pantone be guaranteed?

We get as close as possible through firing trials; the shade approved on a fired piece becomes the series reference.

Why does colour change in firing?

Mineral pigments transform with heat: the final colour only appears after firing.