Guide · Engineering office · 2 min read

Firing porcelain: the stages and the temperatures

A porcelain piece goes into the kiln several times. Each firing has a role: making the piece handleable, vitrifying it with its glaze, then fixing the decoration.

Firing porcelain: the stages and the temperatures

Drying

Before any firing, the piece dries slowly. Drying too fast creates stresses that show up as cracks in the kiln.

Bisque firing

A first firing, at around 900 to 1,000 °C, makes the piece strong and still porous. It can then be handled and glazed: the glaze adheres to a surface that absorbs water.

High-temperature firing

Glaze firing takes place above 1,300 °C, up to about 1,400 °C for hard-paste porcelain. The body vitrifies and the glaze bonds to it into a very hard surface.

Shrinkage

The piece shrinks significantly between the mould and the kiln exit. This shrinkage is calculated from the model stage, and it sets the tolerances of porcelain.

Decoration firings

An on-glaze decoration is fired at around 800 °C; an in-glaze decoration, at around 1,200 °C, sinks into the softened glaze. Precious metals are fired at low temperature, last.

Biscuit

A piece left unglazed but fired at high temperature becomes biscuit: matt, dense and soft to the touch.

How many firings for a decorated piece?

Often three: bisque firing, high-temperature glaze firing, then decoration firing. A gold decoration may need one more.

Why does the piece shrink?

During firing, the body densifies and vitrifies: it loses volume, which the model anticipates.

At our factories

Our kilns in Limoges and at Alföld fire at high temperature; decorations are applied and fired on site, before inspection and packing.