Slip-cast porcelain defects and their causes

Every defect in a cast piece has a cause, in the slip, the mould, drying or firing. Knowing them helps design pieces that are easier to produce and set fair inspection criteria.

Slip-cast porcelain defects and their causes

Cracks

They often start at the base of a handle, in a sharp corner or between a thick and a thin area. Drying too fast or unevenly makes them worse. Radii, even walls and slow drying prevent them.

Warping

At high temperature, porcelain softens slightly: a rim goes oval, a base sags. The shape, the kiln support and the firing curve limit these movements.

Bubbles and pinholes

Air trapped in the slip or released during firing leaves bubbles or small holes in the glaze. De-aired slip and controlled glazing reduce them.

Seam lines

A multi-part mould leaves a fine line on the unfired piece. It is removed during fettling; a well-split mould places it where it shows least.

Uneven walls

Slip of varying density or a mould that is too wet gives uneven walls. Slip control and mould rotation keep production consistent.

Is a piece with a small bubble rejected?

It depends on its size, position and the agreed criteria: the same bubble may be accepted under the foot and rejected on the rim.

Can a crack appear after delivery?

An existing crack is found during inspection, by eye and by sound. After delivery, an impact or thermal shock can cause one: packaging and use matter.

Setting criteria with the customer

Reference pieces, limit samples and inspection level are defined before series production: everyone judges defects on the same basis.

Request a quote